AMiquam Reports 0.1 mm In-Situ Eddy Current Detection in LPBF Thin Walls

The Swiss company's recoater-mounted eddy current sensor is described as detecting 0.1 mm indications in a 0.7 mm stainless steel wall across roughly 127 build layers, with 0.2 mm capability reported in a blade's conformal skin.

AMiquam, a Swiss technology company, is reporting gains in the sensitivity of its in-situ eddy current (EC) inspection technology for metal additive manufacturing, having demonstrated the detection of defects as small as 0.1 mm in thin-walled components produced by laser powder bed fusion (LPBF). The work was set out in a technical publication released ahead of Formnext 2026.

The company frames the development as a shift away from relying exclusively on post-build non-destructive testing to establish component quality, toward inspecting parts layer by layer while they are still being built.

How the inspection is performed

AMiquam's approach integrates an eddy current sensor into the recoater assembly of an LPBF machine. As the recoater travels across the build platform, the sensor scans each newly deposited layer and records electromagnetic signals that can reveal indications associated with internal defects. The inspection data is then mapped onto the component geometry, so that detected anomalies can be located and reported automatically.

Two demonstration cases

  • Thin-walled heat exchanger structures: a 316L stainless steel test specimen with a 0.7 mm wall thickness, into which five holes of 0.1 to 0.5 mm diameter were deliberately introduced.
  • Aeroengine blade structures: an LPBF blade design combining a conformal laser scanning strategy in the surface skin with a conventional chessboard strategy in the bulk material.

In the stainless steel specimen, both through-holes and blind holes produced distinct peaks in the eddy current signal, and even the smallest 0.1 mm indication was described as clearly distinguishable from background signal variation. The measurements were collected across approximately 127 layers, with each hole generating a corresponding signal peak as the build progressed.

AMiquam says the results point to the potential for inspecting complex geometries such as triply periodic minimal surface (TPMS) heat exchangers, where internal channels and thin walls make conventional post-process inspection difficult. The company also outlines a concept for an inspection certificate covering material, layer coverage, detection limits and detected indications, which would give manufacturers a structured record of inspection data generated during production. The certificate shown in the publication is an illustrative example rather than an actual component certification.

Blade results vary by microstructure

In the blade application, the two laser scanning strategies produce different microstructures within the same part, which in turn influence the eddy current signals recorded during inspection. AMiquam reports a detection capability of approximately 0.2 mm within the conformal skin material, while in the bulk material the detection threshold is approximately 0.5 mm, where microstructural variation adds signal fluctuation that makes smaller indications harder to separate.

The company notes that sensitivity depends on material characteristics, laser scanning strategy and component geometry, and suggests that optimising laser strategies could improve detection performance in bulk regions.

Locating indications in three dimensions

Beyond detection, the technology is designed to establish where a defect sits within the part. Signals recorded during each recoating operation are mapped onto the part geometry, and software automatically flags indications that exceed predefined thresholds, assigning their positions in X, Y and build-layer coordinates. AMiquam argues this provides spatial information rather than a general warning of process instability, which can support later investigation into the origin of a defect, and gives manufacturers earlier insight into potential quality issues instead of waiting until the component is complete.

Application-specific limits

The company positions the results as evidence that eddy current inspection could become an integral part of metal additive manufacturing quality assurance, with particular value for complex internal geometries and safety-critical parts. For aerospace, energy and medical manufacturing, where qualification and traceability matter, generating inspection evidence during production could reduce dependence on time-consuming post-build inspection.

AMiquam cautions, however, that detection thresholds remain dependent on component geometry, material and manufacturing parameters, and that the reported figures should be treated as application-specific rather than universal performance limits.

SA

Selin Aydin

Selin Aydin covers calibration, standards interpretation, and instrument procurement across test and measurement, dimensional metrology, laboratory, process, and weighing instruments. Her analysis compares measurement uncertainty, traceability chains, calibration intervals, and life-cycle cost while checking which standards actually apply, such as ISO/IEC 17025 laboratory scope, OIML R 76 for non-automatic weighing instruments, or IEC 61010-1 safety requirements. She helps quality and calibration lab managers, instrumentation engineers, and sourcing teams judge calibration claims, plan verification schedules, and compare total ownership cost before committing to a purchase.